How to Use Polariscope for PET & Preforms to Check Residual Stress | Presto Demo
Prestogroup Online
1 follower
2 Video Views·May 19, 2025
Residual stress can lead to cracking, uneven wall thickness, and bottle failure. In this video, Presto Stantest, Asia’s No.1 testing equipment manufacturer, demonstrates how to use a Polariscope to inspect PET preforms and bottles for internal stress. Ensure dimensional stability and avoid defects before blow molding begins. Contact us at +91 9210 903 903 or [email protected] for premium quality testing instruments tailored to your needs.
For more information visit our website: -https://www.prestogroup.com/categories/polariscope/
Today we will be discussing about a very important instrument that is polariscope which is very
useful for the pet and preform industries.
So the polariscope we will look today is mainly for this kind of industry, the pet sheets,
pet bottles and the preforms.
So the purpose of a polariscope is to see the residual stress in the sample which we
cannot see through our naked eyes.
So if I talk about a standardized thing in this, so it follows the ASTM D4093 standard
which says for a polariscope to measure the residual stress in the sample.
So the analysis we will be getting is visual and if I talk about the principle, it works
on birefringence principle which says for double refraction when I will switch on the
two light source.
So this is the area from where the light will glow and the sample will be placed here.
So if the stress is there in the sample, so it will show in the form of colors and it
will split in two different rays and it will show you different different colors.
So each color depicts a certain level of stress in the sample.
The lighter depicts less stress and the darker depicts more stress.
So this is how we will be analyzing the sample.
So I will be taking an optimum and non-optimum sample.
So right now the samples I have, I don't know that which sample after the manufacturing
stage is a good sample or a bad, but we can see through this polariscope.
So these two sample I will be checking.
So one, if I see this sample through naked eyes, I can see that there is no stress in
the sample.
It is a perfect looking, but how it will look in the polariscope will show you the stress
level in the sample or how much optimum it is.
So this is one.
Now I will be taking this small preform and I will check that how optimum this sample
is in the 90 degree orientation and 45 degree orientation.
So now we will be discussing about the labeling of the machine.
So starting with this panel, so we have two light sources in this.
First is this CFL light source, the second is sodium lamp light.
So when we will switch on these two light source, we will get the polarized light, a
monochromatic light which will not disperse here and there and will come in a straight
line and we will be able to get the accurate stress analysis.
Other things here, this area is known as polarizer where we place the sample.
We also have a template at 90 degree and 45 degree orientation.
Then from the area which is a viewing glass from where we used to see the residual stress
in the sample.
So this is the part, this is known as analyzer.
So now we will be observing the sample at two angles, 90 degree orientation and 45 degree
orientation.
So this is the analysis at 90 degree orientation and we will shift it to 45 and we will be
able to see that this is one of the optimum sample.
So you will be looking at the color, the colors will appear on the sample to show that the
stress is there in the sample because this has been folded.
So you will be looking at the stress and the colors on the side walls.
So how uniformly the stress is distributed.
So that matters a lot in the process.
So in this sample we can see that stress is distributed very properly.
If the blue line is coming on this side, on this side, so it is also coming on this side.
If it is coming on this corner portion, so it is also coming here.
So this is how an optimum sample looks like.
Now let me show you that how a non-optimum sample looks like.
So this thing we will not be able to see through our naked eyes, this sample.
So now if I place it here at 90 degree orientation and if I will be placing it here now.
So here we can see on this particular side, you can see that the stress has distributed
a lot on this surface.
So this was not seen in this big preform.
So this is how a non-optimum sample looks like.
It means there is a lot of stress on this particular surface.
So during the manufacturing process there is some sort of defect in the sample.
So the process we have to rewind again and whatever the issue is, either it is because
of excessive thermal energy we have given or it is whatever the process is, so that
we have to check.
So the solution is something that the person who is doing the process they knows.
So it is very important to understand that which is the part which is having an issue.
So that you will be able to analyze through this particular instrument.
So this is how you can analyze the defect in PET sheets also or any kind of PET preforms.
Thank you so much.