The radial drill project has left me with a lot of chunky cast iron parts that need de rusting. Its the perfect time to try something I've been meaning to try for ages - Molasses as a liquid rust removal solution.
This is how I went about cleaning up all these incredible gears, shafts and pulleys, and I'm pretty pleased with the results!
Bit of a short one today but I don't want to waffle on too long!
Follow my Instagram for regular project updates and what ever else happens to be going on!
/ iron_jonsey
Using ordinary feed molasses as a rust dissolving liquid dip, does it work? Yes.
All of these parts a few weeks ago were in an absolute state.
They're all off of my radial drill project. This is just a small selection
and if you've been following along you will know what these look like.
This is one of the racks that is used to traverse the drilling head up and down the arm.
That has come out so well. It's even pulled out the rust from the pitting and inside the teeth.
These chunky gears, comb, back gears, bevels all come out really nicely.
This is probably my favourite. This is the shaft that drives the worm and wheel set that
raises and lowers the column. The way that's pulled all the rust out of there is really
impressive. Now you should all recognise this guy. This is the pinion that again raises and
lowers the arm. This was quite possibly one of the rustiest things I've ever seen in my life.
Just look at how nicely that has come up. So I don't think whether it works or not
is really up for debate. So what this video is going to be about is how does it work,
why I decided to use it, how long does it take, how bad does it smell and will I use it again?
All of these parts have been thoroughly degreased and washed. Any paint, grease or other muck will
stop this process working so well. I'm stacking the parts in the bottom of the barrel in a bit
of a haphazard nature to try and avoid as much part to part and part to barrel contact as possible.
In an ideal world the parts would be suspended in space completely surrounded by the solution,
but because that's impractical we are going for the jumbled pickup sticks method. The container
has to be plastic otherwise the mixture will attack it so you can't use that rusty old oil
barrel or your aluminium beer keg. Apparently the mixture will eat non-ferrous too. I haven't tested
that personally. I certainly won't be risking any bronze bearings that's for sure. Once everything
is in it's time to dump in the molasses. I bought this 25 litre tub from my local farm store and I'm
throwing in the whole lot. The capacity of the blue barrel is about 220 litres and it won't be
full so we will end up with a mix somewhere around one part molasses and seven parts water. I agitated
the mixture as best I could but the molasses actually dissolved into the water easier than
I thought it might. So fast forward now and the parts have been soaking for two weeks and it is
definitely time for a clean. I was aiming to remove, scrub, wash and return everything to the mixture
once a week, but I got busy with other things and kind of forgot about it, so here we are. The
mixture had developed a lot of surface gunge which needed to be scraped off the top before removing
the parts for inspection. All of the parts received a rinse with water and a clean with a wire brush.
The reaction leaves a black residue on the surface of the parts and once this forms it actually
creates a barrier stopping the mixture from working on rust that may be lying deeper on the part.
It's essential this residue is mechanically removed so the mixture can attack fresh rust
underneath it. On this first wash the areas where the rust was light had come up great but there
were still spots of deep rust and rust staining that needed another soak. So it was good to see
that the mixture was working properly, although it definitely required a bit more time. Some parts,
namely some of the shafts, which weren't that exposed on the machine came out really well
after the first soak, so I didn't bother returning them to the bath. One thing to note is that the
black residue formed by the molasses seemed to be harder to remove than the same residue from
some of the commercially available rust removers that I have previously used. I'm not sure why,
but it is something I definitely noticed and added quite a bit of time to the process. It could just
be that these are extra heavily rusted components but I'm not too sure. I took this video a day after
replacing the parts back in the bath. It's amazing how quick it starts to work and how you can almost
see the rust dissolving, creating a shadow of the parts below on the surface of the mixture. Now fast
forward again another two weeks and the parts have had a full month in the molasses mix. It's time
once again to pull out the parts and give them a thorough rinse and clean. I find that a combination
of an angle grinder with a cut brush and a die grinder with a mini wire wheel work wonders for
this kind of cleaning. The grinder is perfect for covering large areas quickly while the die grinder
is ideal for reaching the troughs of gear teeth and other small spaces. My process is rinse,
wire wheel, followed by a further rinse, dry off with a rag and a good spray of WD-40. The WD-40
is perfect for driving out excess moisture and providing a film of oil to prevent flash rust.
All rust dissolving processes leave iron so clean that it will flash rust immediately on contact
with oxygen, so this oiling step is vital. You can submerge freshly cleaned parts in clean water to
isolate them from oxygen in the air and there are also additives available to add to said bath
which prevents the flash rusting. This is only really handy if you plan to paint parts after
de-rusting and so don't want them covered in oil. Once I've built up an amount of clean parts I'll
then coat them all in machine oil which will protect them enough on the shelf until we get
round to reassembling them back on the machine. For gear teeth like this pinion which has sides
and so very difficult to clean with a circular wheel, I like to take an ordinary mini brush,
literally grind it into a point and it becomes a really handy pointy spinny thing that can reach
into all the nooks and crannies. The molasses and water solution works to dissolve rust because of
a thing called chelation. The molasses contains a wide variety of naturally occurring amino acids,
some of which are chelating agents. When in contact with the iron oxide, which of course is rust,
these chelating agents, by some magic of chemistry which I don't really understand,
surround and bind onto the iron ions, that's weird to say, in the rust and thus separate
them from the base metal, allowing them to be easily washed away by the water in the mixture.
Molasses is made from sugar beet and it's presumably these amino acids that allow the
plant to absorb iron and other metallic minerals from the soil when it is growing, and perhaps
they help the cattle who are fed the molasses absorb the same minerals. Anyway I'm not a sugar
beet plant nor am I a cow, I'm an old iron enthusiast who can take advantage of this
natural process to make some 19th century cast iron parts shiny again. Now the biggest and probably
the most interesting part is lurking at the bottom of the barrel, the cone. This is the main driving
pulley for the drill. We removed it back in part two along with its shaft and back gears. It's
known as a cone pulley because of its shape caused by its four steps descending in diameter.
There is meant to be another cone identical to this which when mounted on a counter shaft in
the ceiling in line with the cone on the machine but flipped the other way around, a single belt
may be moved about the four steps. When the counter shaft is driven from a line shaft or another form
of motive power we can gain four distinct speeds using the steps by shifting the belt between them.
This other cone is obviously missing and making it again from scratch is going to be one hell of
a challenge on this project. Luckily it doesn't need to be as complex as this cone, the features
such as the pinion on the small end for the back gears and also the belt flanges are all unnecessary
for a counter shaft cone. It's just the widths and the diameters of the steps which need to be
identical. This is one hell of a casting, of course it's mostly hollow so there must have
been some interesting cores involved in the mould box. I mean look at the three support struts inside
just to give the whole thing strength in line with the three notches that allow the cone to be engaged
and disengaged from the driving ball wheel. More on that when we reassemble it in a future episode.
Plus the pinion on the end which is all part of the same casting and the teeth aren't machine cut,
none of the gear teeth on this machine are, they are all cast in. I'd have loved to have been in
the foundry that day to see exactly how they moulded up some of these parts. All that's left now
is to scrape the bottom of the barrel for the last smallest parts. All the random nuts bolts which I
hope I can remember where they go and the strangely shaped bearing piece which came off the very top
of the spindle. So would I do it again? Yes, but only in very specific circumstances. It definitely
has its place but I don't think it has many places. It's obviously extremely cheap so I
mixed up that blue barrel for less than 35 quid. Evaporust or any of the other commercially
available liquid dips just can't even come close to that cost-wise. The other big
advantage is that it is obviously completely organic, it's just sugar. It's safe to deal with
and very easy to dispose of. That's pretty much it for upsides to be honest because it's
extraordinarily slow. I mean it takes weeks unless you've got it in a heated environment or you put
in an immersion heater or something like that. But then some of the cost savings go out the window.
I've done it in the British spring time which has been unusually warm so it's been between
15 and 25 degrees over the last few weeks. I specifically waited until this time of year in
order to do it. There's no point doing it when it's below 10. It smells, it smells horrendous.
It was all right for a few days but once it got going it got going. So if you have to do it in
your main workshop where you're functioning most of the time then I wouldn't do it. If I had to do
it in here then I wouldn't do it because on hot days when that got going it was difficult to exist
anywhere near it. Luckily I have a lock up next door which is kind of a storage area so I was able
to do it in there. But even so I am backwards and forwards. It was a little bit unpleasant
to be around. Maybe adding a lid would probably help. I don't know whether that would inhibit the
infectiveness or not. Removing the oxygen supply. Whether it likes to have a constant supply of
oxygen to keep the reaction together. I don't know. I'm not a chemist. Maybe someone can tell me that.
But for large chunky parts where you have a lot to do and they take up a lot of space it's a really
good way of mixing up a lot of solution very cheaply and put it in a corner and forget about
it for a month or so or longer. Then it's the perfect solution. Obviously there's other things
like electrolysis and other organic based methods like citric acid and various concoctions of that
and other things. I've not tried any of those but I just settled on molasses because I've heard about
it online and I thought I'd give a crap. I'm very pleased with the results. It was a bit of a faff
but got there in the end and really excited to be moving along putting the rest of the drill
together. I hope you'll join me for that. Thank you so much for watching and I'll see you in the next one.