In a historic scythe forge in Germany, craftsmen carry out a rare and demanding repair: replacing the hammer stock, the massive oak foundation that supports a traditional forging hammer. Buried deep in the ground, this oak trunk absorbs the shock of thousands of hammer blows as blacksmiths shape scythes and sickles. The process takes days of careful work. The old, worn foundation must first be uncovered and removed. A new oak trunk is prepared, fitted with a heated iron ring, and lowered into the pit. Layers of wood and earth are packed around it to cushion the hammer’s impact before the forging hammer is rebuilt and tested again. These large mechanical hammers were once the heart of many European tool factories. Before modern pneumatic machines, they powered the forging of agricultural tools and blades through simple but powerful mechanical systems. Maintaining them required skilled blacksmiths, hammer masters, and carpenters who understood both wood and iron.
Craftsmen at the Freudenthal Scythe Forge in Germany restore a traditional helve hammer by replacing its massive oak anvil block. The process involves precise measurement, traditional woodworking, and meticulous reassembly to ensure the hammer can perform the delicate planishing work required for sickle production.
Long before pneumatic hammers,
the rhythm of the forge was driven by water and wood.
In today's Aged Skills History episode,
craftsmen at the Freudenthal Scythe Forge in Germany
repair and reinstall the massive hammer stock
of a traditional tail hammer,
renewing the wooden foundation that absorbs
the force of thousands of forging blows.
The Hammer Master, a trained scythe smith from Austria,
starts by measuring the old assembly.
Recording the distance between the anvil cap, the hardened
steel anvil set into the top of the block, and the shop floor.
The height alone is not enough.
The angle between the anvil cap
and the hammer frame must also be noted precisely,
so that when the new block is set with the hammer out of the way,
everything lines up exactly as before.
One more factor has to be accounted for.
The block will settle by roughly two inches after installation.
With all measurements carefully recorded,
Hermann Schmid and Hermann Zimmermann begin
stripping out the helve, the hammer's complete working assembly.
It consists of the wooden
helve shaft together with the iron and steel fittings,
the rocker, the beam, and the hammer
head. To free the helve from the frame,
the rocker wedges, called packing irons, are first driven
loose with sledgehammers.
These wedges are locked into the hammer uprights by means of hardwood
Wood Packing Blocks
The two smiths work
the helve free until
it can be swung clear
and set aside. Before
the helve shaft
can be pulled out, the anvil cap
and lower die saddle must first be lifted out of the anvil
housing. The
hammer being
overhauled
here is the last
of six helve
hammers
that were still
running
as late as 1957 before giving way to pneumatic and spring hammers.
Pneumatic hammers had in
fact been arriving at the forge since 1926,
brought in to handle certain finishing operations.
This particular hammer was acquired in 1960
from a scythe works in Hagen, where it had already been
returned to regular production use.
At the Freudenthal forge, the Helve hammer handles the
planishing work, the final smoothing passes
in sickle production.
Using pieces of red hot iron,
the
retaining
hoop
that will
be reused on
the new anvil
block is now
worked loose.
When the
assembly is fully rebuilt,
are used to burn away the hardwood packing wedges holding it in place.
Once charred through,
the packing blocks can be pried out with a crowbar.
With the packing cleared,
the anvil cap can be lifted free from its socket in the top of the
block, burning out. Clearing
and pulling the anvil cap alone takes well over an hour. The full job,
pulling the helve, removing the cap,
digging out the old block and setting the new one true,
runs to two full working days, with two men on the task throughout.
With the helve and anvil cap out of the way, the old anvil block,
buried roughly three feet deep in the foundation,
can now be worked free.
Meanwhile, on the other side of the yard,
the new block is being readied.
The horse manure needed for the bedding has been set out.
The oak trunk, roughly eight feet long, has already been dressed round.
The hammerite now has to cut the socket for the anvil cap
into the top of the trunk and confirm it is dead plum.
The oak log used for this block was bought around 1972
from a sawmill in the Bergisches
Land hill country, and has been seasoning in the yard ever since.
In the Rhineland, the an-
In those days, treating the wood
with preservative was not yet common practice.
The iron hoop has to be heated before it can be driven on.
The right temperature is around
400 degrees Fahrenheit,
reached after about an hour and a half in a hardwood fire.
At that heat, the hoop grows by nearly an inch in diameter,
just enough to slip over the oak trunk.
If it ran any hotter,
it would spring back under the mallet and refuse to seat.
Water is poured
over the hoop
not only to keep
the wood
from scorching,
but to quench the iron quickly
so it shrinks down hard around the trunk.
The hoop,
roughly six
and a half
feet around
and four
inches wide,
is hammered home until it grips under full tension.
The smith can tell it has seated
when it gives a clear ring under the hammer.
In earlier times the hoop was often fitted inside the workshop,
heated in the same forge fire used for tool work
or for hardening the hammer dies.
While
the
new
block
has
been
taking
shape
in the
yard,
the crew inside has
been digging
the old worn out
anvil block free.
It quickly becomes clear that the old block had
been failing for some time.
It is nearly rotten all the way through.
Normally the heartwood should remain sound,
decay usually works inward from the outside
rather
than
starting
at the
core.
Once the
block is
hauled
out of
the pit
on a rope,
exact dimensions can be taken off it for sizing the replacement.
The
prepared
oak
trunk
is now
trimmed
to the
required
length
of 63
inches,
while the
slow work
of fully
clearing
the pit
continues
alongside.
Provided
the wood
has not gone too far, the old block will
be passed along to the smiths for firewood.
Spent oak always made a welcome addition to the fuel pile.
With the
groundwork
done,
the two men
have worked
the pit down
in two
stages.
Before the new block can go in,
every last scrap of old timber must be cleaned out of the pit to
give it
a proper footing. A bed
of small-diameter logs
and horse manure is now
laid at the bottom
This particular bedding method was a Rhineland tradition.
Elsewhere, the block might be set on crushed stone
or cast directly onto a concrete pad.
For the two
log layers,
softwood
poles three
to four
inches
across
and cut
to roughly 30
to 40 inches
long are used.
In the old days, the block had to be dug up every four
or five years to replace the rotted bed logs.
Nowadays, the block is simply left undisturbed until
the oak itself begins to fail, which takes roughly 14 to 15 years.
The new block, trimmed to length
and given a coat of modern wood preservative,
is now lowered
into the pit. Chalk
lines marked along
the side of the trunk,
and directional arrows drawn on top give
the crew reference points for getting the block
properly oriented as it goes in.
Until 1926, the Freudenthal forge
ran entirely on Helve hammers.
They were phased out one by one
because of their relentless maintenance demands.
On any given day, one or two hammers were down for repairs.
The firm kept two full-time wheelwrights
on staff,
whose only
job was to
maintain
the hammers
and anvil
assemblies.
Once
in the pit,
the oak trunk is plumbed up
and held firmly in position with wooden shore props.
Into the bored socket at the top of the block, roughly 16 inches deep,
the anvil cap, which can weigh up to 100 pounds, is lowered into place.
Before the cap is driven home, the hammer master checks
its position against the measurements taken at the start of the job.
With the cap seat,
the remaining gaps around it are packed
tight with tapered hardwood wedges.
Only sound, straight-grained stock is used.
For the past 30 years, self-setting taper wedges have done the job.
Once the cap is fully secured,
the Hammer Master takes a final measurement to confirm the block
has not shifted. Any small deviation can still
be corrected at this stage by tapping the shore props,
walking the block
into its final position.
With the cap wedged tight,
the ends of the packing
wedges
that stand proud
are trimmed off flush.
With the block set
true and the anvil cap
in place,
the crew honors the old craftsman's tradition.
A brief topping out to mark the completion of
of the new foundation.
With the ceremony done,
the men set to work filling
the pit back in.
The wooden tamping block
used here to pack the continuously wetted earth in the pit,
about four and a half feet wide and
four feet deep, was made specially for this film.
On a normal job, iron rammers would be used
throughout.
Tampers
shaped
to cradle
the curve
of the anvil
block were
standard
shop
equipment
Back when the current Hammer Master was serving
his time at Scythe Works in Austria.
Seated on the underside of the hammerhead is the replaceable top die,
which works against the
bottom die saddle seated in the anvil cap,
the two together forming the matched working pair.
The tail end
of the helve sits
the hammer pole,
a heavy iron block
whose weight sets the striking force of the hammer.
Using a chain hoist, a block and
tackle would have been used in earlier times,
the helve is lifted back into the hammer frame.
The first step is to fit the pivot journal into the bearing bore
of the right-hand rocker arm, which is held in the hammer upright.
Once the rocker is settled in the bearing block
with its hardened journal in place, the left-hand rocker arm
is slipped onto the journal and pushed home into the upright.
Each bearing block offers three conical sockets,
each about an inch deep.
As one wears out, the journal moves to the next,
extending the life of the bearing.
Both bearing blocks are then locked down
with hardwood wedges and iron shims,
the same packing irons used
earlier. With the helve back
in the frame,
the anvil cap and bottom die saddle can
be reinstalled in the anvil housing.
The bottom die carries the hardened lower working face
and is designed to be swapped out when worn,
held in place by the iron anvil cap that surrounds it.
Once the hammer is roughly set up, the dies are dressed.
The Hammermaster does it himself here,
though in normal shop practice, each smith ground his own dies.
All dies are finished by hand, usually with a power grinder.
The face of a planishing die is rectangular,
with a slight crown running both along and across its length.
Because of the wear involved, planishing dies need
to be re-ground after every 1,000 to 2,000 pieces struck.
Final dressing of a die takes about 10 minutes.
The bottom die saddle can then be fitted back
into the anvil
housing.
The top die
is set with a
slight offset
to the right of
the bottom die.
This is critical for planishing work,
where the smith needs to smooth both the face of the blade
and its back edge
in a single pass.
With the new block in place
and everything reassembled,
the hammer is ready
for its trial run.
During the run-in, the striking
alignment can still
You can still be fine-tuned by tapping the shims.
Once the hammer is falling in a steady even beat
the trial is properly underway. The drive fork
picks up the rotation
from the line shaft
and carries it
to the cam wheel.
Power reaches the
hammer through a belt drive off the overhead line shaft,
the standard arrangement in workshops of
this era. The first forging
passes will reveal whether
the hammer is set up to the closed
tolerances that blade work demands.
Planishing is one of the final operations in bringing a scythe
or sickle to finished form.
Watch how the blade is walked across the die face seven
or eight times from shank to tip,
tracking the arc
of the hammer's stroke.
With each pass, the blade,
already forged to rough shape in earlier heats,
is drawn out a little further,
pushed forward along its length,
spreading slightly toward the shank, while the steel
is consolidated and the grain refined.
By the time the last pass is made, the blade is ready.
After the block has had 14 days to finish settling,
the pit can be fully backfilled.
Before that, the top and bottom dies will need one final grind
and the strike alignment checked once more.
Only then will the hammer be cleared for full production.