Izod Impact Test | ASTM D256 | Impact Strength Testing of Plastics Explained in Detail
Prestogroup Online
1 follower
4 Video Views·Feb 20, 2025
In this video, we explain the Izod Impact Test (ASTM D256), a crucial method used to determine the impact resistance of plastic materials. This test helps manufacturers assess the toughness and durability of plastics under sudden impact forces.
For more information visit our website:- https://www.prestogroup.com/products/izod-charpy-impact-tester/
Hello everyone, the topic of today's discussion is about IZOD impact strength test.
So, IZOD test is to judge the impact strength of any type of polymers like nylon 6-6, polypropylene, ABS, HDPE, LDPE.
So, we can judge the impact strength of any type of polymers through this particular machine.
We can judge the impact energy consumed by breaking a particular plastic sample and that too by standardized method.
So, this particular machine is made properly as per ASTM D256, in which its length of pendulum, its principle of working, specimen preparation, everything complies with that standard, even weights.
So, we will discuss it one by one.
The working principle of the machine is as per ASTM D256, cantilever beam type IZOD impact strength is its mechanism of working.
And the length mentioned for pendulum is 265 mm.
And the angle of striking that we have to maintain at the initial stage or its calibration is 150 degrees.
So, now let's discuss about weights.
So, in ASTM D526, it is mentioned that weights should be provided from 21.71 joules to 21.7 joules.
So, while maintaining that, PRESTO provides R1 weight, whose weight is 2.71 joules per meter in R1.
R2 weight is 5.42, R3 weight is 10.84 and R4 weight is 21.68.
So, this is the combination of all the weights.
So, now let's talk about specimen preparation because it is a very important parameter in testing.
We have to make specimen as per standard if we want an accurate testing.
So, length wise, 63.5 will be the length of this sample and 12.7 will be its width.
We have to prepare a notch in it for which you can use PRESTO notch cutter.
In which we have to prepare a notch of 2.54 mm.
I am telling you its depth.
And when you maintain the depth of 2.54 mm, then the remaining should be approximately 10.6 mm.
Its depth after making notch.
So, all these things are mentioned in the standard.
And its thickness will be lower limiting value from 3 mm to maximum 13 mm.
So, this is IZOT 4P impact tester.
So, this is its digital control panel because this is a digital model.
In this, we have to feed some parameters before starting the testing.
So, this is the CAL button, we will press it.
And here it will show how many joules we are testing.
Which particular energy weight we will use to properly strike our sample.
So, now we are using R1 weight.
Next, we will go.
We will press PAR, P-A-R.
And here it is depicting which symbol, which weight.
R1 depicts 2.71, while R2 depicts 5.42, R3 10.84.
It works like this.
Next, we have to feed the sample thickness.
On which particular thickness we are testing.
We will feed that thing.
So, now the thickness is 3.40.
And now we will come to our panel and proceed with the testing.
So, for safety purposes, this magnetic door is also provided.
So that when the sample breaks, it is not outside or harms anything.
So, now we will open this door and understand the sample placement.
So, in sample placement, there is a very important difference between IZOD and Charpy test.
What we are performing now and the fixture used is according to the IZOD test.
Here I will place the sample.
And we will place the sample vertically.
In Charpy test, the sample is comparatively longer and is placed horizontally.
And its fixture is also according to that.
And the best part is that you can close it on a fixed torque.
For example, here it is labelled in Newton meter that how much force you have closed it with.
So that you close all the samples with the same force.
So, this is also an important thing.
So, now we have placed the sample.
And now we will close this magnetic door.
That is for safety purposes.
Now we will start the testing.
I will press this manual release button and this pendulum will strike.
So, our testing is complete.
Now we have to see the result.
Here, the reading below is 0.690.
This is shown in Joules per meter that how much energy our sample has consumed while breakage.
And the reading above is 113 degree.
This is the angle.
This is the angle of striking when the sample was breaking.
So, this is the angle and this is the energy consumed while breaking.
So, this is how we calculate the impact energy.
So, this is 0.690 Joules per meter that the sample has consumed while breaking.
So, I will remove the specimen.
So, now this sample has consumed 0.690 Joules per meter while breaking.
It means that if a sample consumes more energy than this,
then obviously its quality would have been comparatively better or it would have been able to sustain more load.
If something is being placed on it or if there is some impact on it.
So, this thing we know from this machine.